Abstract
After severe plastic deformation by high-pressure torsion, the density of grain boundaries is so high that in HRTEM images frequently moiré patterns occur open to misinterpretation. The observed dislocation densities are far too low to cause homogeneous destruction of long-range order and homogeneous amorphization in Ni3Al and NiTi, respectively. Œ 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
| Originalsprache | Englisch |
|---|---|
| Seiten (von - bis) | 789-794 |
| Seitenumfang | 6 |
| Fachzeitschrift | Scripta Materialia |
| Jahrgang | 51 |
| Ausgabenummer | 8 SPEC. IS |
| DOIs | |
| Publikationsstatus | Veröffentlicht - 2004 |
ÖFOS 2012
- 1030 Physik, Astronomie
Fingerprint
Untersuchen Sie die Forschungsthemen von „HRTEM analysis of nanostructured alloys processed by severe plastic deformation“. Zusammen bilden sie einen einzigartigen Fingerprint.Zitationsweisen
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver