Abstract
The transformation of schwertmannite to goethite was studied by ageing one
synthetic and five natural schwertmannites in water at room temperature. Additionally, one synthetic
and two natural schwertmannites were kept at variable pH (2, 4, 6 and 8). After one year, only the
synthetic sample and one natural schwertmannite had transformed to goethite. However, the oxalate
solubility of Fe and trace elements in all the samples decreased, whereas the total Fe/S ratios and
specific surface areas of all samples increased. Arsenic and organic matter appeared to suppress the
schwertmannite-to-goethite phase transformation. At pH 2, synthetic schwertmannite fullytransformed
to goethite, but at pH 46 only minor transformation occurred. Depending on pH,
many trace elements were released into solution during ageing of the natural schwertmannites. In
general, Co, Mn, Zn and Si were released to solution, whereas As was enriched in the remaining iron
oxide fraction. Al was dissolved at pH
| Original language | English |
|---|---|
| Pages (from-to) | 437-448 |
| Number of pages | 12 |
| Journal | Clay Minerals: journal of the European Clay Groups |
| Volume | 43 |
| Publication status | Published - 2008 |
Austrian Fields of Science 2012
- 105904 Environmental research
Fingerprint
Dive into the research topics of 'Ageing of synthetic and natural schwertmannites at pH 2 - 8'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver